Customization: | Available |
---|---|
After-sales Service: | Online Support |
Type: | Rotating Anti-Bending and Straightening Machine |
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Model | MHT40-400-21 | MHT40-800-21 | MHT40-1300-21 | MHT40-1600-21 | MHT40-2100-21 |
Width | 0-400mm | 0-800mm | 0-1300mm | 0-1600mm | 0-2100mm |
Roll diameter | 40 | 40 | 40 | 40 | 40 |
Rated thickness | 0.6-3.0mm | 0.6-3.0mm | 0.6-3.0mm | 0.6-3.0mm | 0.6-3.0mm |
Maximum thickness | 6.0 | 6.0 | 6.0 | 6.0 | 6.0 |
Number of rolls | 21 | 21 | 21 | 21 | 21 |
Shortest part | 70 | 70 | 70 | 70 | 70 |
Leveling speed | 0-10m/Min | 0-10m/Min | 0-10m/Min | 0-10m/Min | 0-10m/Min |
Voltage | 3-phase 380v | 3-phase 380v | 3-phase 380v | 3-phase 380v | 3-phase 380v |
Optional | 1.Loading and unloading and reclaiming munipulators 2.Loading and unloading joint robots 3.Automatic detection platform 4.inlet and outflow assembly line 5.Automatic stacking lifting platform 6.Roller quick cleaning device |
Other Similar models:
Normal MHT CNC High precision Leveling Machine | Model code | Roller Diameter(mm) | Thickness (mm) | Width(mm) | Roller qty(Standard) | Shortest part(mm) |
MHT10 | 10 | 0.03-0.6 | 100-300 | 31 | 20 | |
MHT15 | 15 | 0.08-1.0 | 100-600 | 31 | 30 | |
MHT20 | 20 | 0.3-1.2 | 200-1600 | 23 | 40 | |
MHT30 | 30 | 0.5-2.0 | 400-3000 | 23 | 60 | |
MHT40 | 40 | 0.6-3.0 | 400-3000 | 21 | 70 | |
MHT50 | 50 | 0.8-4.0 | 400-3000 | 19 | 90 | |
MHT60 | 60 | 1.0-6.0 | 400-3000 | 21 | 100 | |
MHT80 | 80 | 2.0-8.0 | 400-3000 | 19 | 130 | |
MHT100 | 100 | 3.0-12.0 | 400-3000 | 19 | 160 | |
MHT120 | 120 | 4.0-16.0 | 400-3000 | 19 | 190 | |
MHT150 | 150 | 6.0-25.0 | 600-3000 | 19 | 240 | |
MHT200 | 200 | 8.0-30.0 | 800-3000 | 15/19 | 310 | |
MHT250 | 250 | 10.0-40.0 | 1000-3500 | 15/19 | 390 | |
MHT300 | 300 | 12.0-50.0 | 1000-4000 | 15/19 | 480 |
Problems may occur when processing unleveled coils
Roll forming
During rolling molding, a roller is used to change the shape of the steel sheet coil through a series of processes. The defects of stress and flatness of raw materials make it difficult to realize accurate forming of coil. Due to the fast processing speed, the roughness defect of the roll will bring serious negative impact on the processing safety of the rolling molding line.
Stamping
The flatness defects and internal stresses in the coil can make accurate forming difficult. On the one hand, it may cause
mold damage, on the other hand, it may lead to a decline in the quality of finished products. In addition, the flatness defect of raw materials may also cause the whole equipment to stop running and reduce the use efficiency of the equipment.
Shear plate
Shear processing will release the stress in the raw material, resulting in visible deformation of the material. The flatness defect of the coil will not guarantee the shear precision. The flatness of raw materials is a very important quality standard,because the sheared sheet is usually processed in a subsequent process.
Laser cutting line
Whether it is from sheet material, coil material to finished product, highly automated integrated processing line, smart factory, etc., the flatness defect of the coil material will not guarantee the cutting accuracy and is more likely to cause the loss of the laser head. After high-precision leveling It can improve efficiency and precision faster, save time and space,and reduce the cost of raw materials and accessories.
Deburring production line
In the process of deburring, the unevenness of the workpiece will lead to a decrease in the quality of the part. Some parts cannot completely remove burrs or iron slag. After leveling, the workpiece can quickly improve the efficiency and quality of deburring and reduce the rework rate and rate.